Jig requirement for anodizing?





2005

Dear Sir or Madam
Two questions on jig need your help:

1. Rustless steel could be used for jig preparation?
Our jig was made of two parts:
Hook: Titanium
Other part: Rustless steel.

2. Insulation
is it permitted to use a paint film in the jig surface?
If not, why?
The jig we prepared was covered with some PVC paint for insulation.
But some expert said it was a nightmare for maintenance.

Qiang Luo
Yida - Shanghai, China



Properly applied PVC plastisol coatings are not a nightmare at all; they have been successfully used on countless thousands of electroplating racks for decades. Still, it is usually more economical and practical to make anodizing racks of titanium or aluminum than of plastisol coated stainless steel. Besides, stainless steel has low current-carrying capacity--about 1/5 of aluminum.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.
2005


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"