Need general info about Electroplating process for school




Hello, I've been searching for days and honestly, I'm not very good on computers and I have a very important [paper on ELECTROPLATING....... So I really need as much info/sites as possible. Please help me! Anees H.

Anees Harb
- Muscat
2000



Just start with our FAQs, Anees Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.
2000



DEAR SIR

I need the information about the ELECTROPLATING process for zinc and nickel plating. KINDLY PLEASE SEND ME THE INFORMATION REGARDING THE EQUIPMENT,CHEMICAL COMPOSITION USED IN THE PROCESS.

MANISH VISHWAKARMA
M/S M.S.ENGINEERING - INDIA
2005



Hello Manish. That sounds like a simple request, but it isn't. It took me many more years to become marginally knowledgable about zinc and nickel plating than it took me to acquire my engineering degree, and I don't think it will be different for you. Start with our "must have" booklist. Good luck.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.
2005



Please let me know how to electroplating Cs to Cu.

Tri Murni
Indonesian Nuclear Energy Agency - Jakarta, DKI Jakarta, Indonesia
2003


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"