Buffing and polishing




What are Non Woven Buffing Wheels?
Where are its uses? What type of Polishing do we get in Non Woven Buffing Wheels?
Please give details.
Thanks

ASHOK MALLUR
Polishing - Bangalore, KARNATAKA, India
2005



Almost every good abrasive supplier should know or be aware of non-woven wheels and belts. These are made from a combination of densely packed synthetic nylon/alum impregnated fibers.

tony kenton
AF Kenton
retired business owner - Hatboro, Pennsylvania
2005


The wheel which was densely packed by the strips which was made up of Nylon Fiber & abrasive grains (or) cloth/paper backing with abrasive grains

Jaya Prakash.V
- Chennai, Tamil Nadu, India
2005



Non Woven Abrasives are three dimensional abrasives, instead of the normal two dimensions that are available with coated abrasives.

Density of the Non Woven Abrasives should be selected only as per your preference.

Regards,

Nitesh Kedia
- Mumbai, Maharashtra, India
2005


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"