Zinc Dichromate


1999

Hello,

I'm relatively new to the Web so any help that you could give me would be appreciated.

What does Zinc Dichromate involve? What basic chemicals are used? Is it similar to electroplating?

The reason that I ask is because I run a hard chroming plant and I'm wondering what the costs might be to start a Zinc dichromate branch! Thank you for any help/direction you might be able to give me!

James

James Corbeil
Ontario, Canada


1999

Hi James , If you mean by Zinc Dichromate , A yellow finish over Zinc Electroplate, then the man to talk to is Ken Lemke of Canadian Finishing Systems, who are located in Burlington Ontario and are attached to this site under suppliers .

regards

John Tenison-Woods
John Tenison - Woods
- Victoria Australia



If you have a question in mind which seems off topic, please Search the Site

ADD a Q, A, or Comment on THIS topic START an UNRELATED topicView CURRENT HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2019 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.