Would like to know a chemical or other method to remove zinc from the surface of brass leaving the copper behind. Is it possible to do this without destroying the surface finish?

Mandar Sunthankar
- Fort Collins, Colorado


(2000)

Respected Sir I am a student at IIT kanpur doing master of technology Since I would like to the etchant solution and its mode of preparation for etching zinc. So Sir I kindly request you sir to send me the solution for the above query. Expecting your reply. Thanking you Sir, Yours sincerely

Nacham Sridhar
Indian Institute of Technology - Kanpur



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.