Copper plating on graphite fibers


(1999)

I am looking for a company for plating Copper on graphite fibers. We would like to coat 0.05, 0.1 and 0.5 micron Cu on: IM7 fiber (HEXCEL, tensile strength 5308MPa, 5 microns in diameter) or IM9 fiber (HEXCEL, tensile strength 6343MPa, 4.5 microns in diameter) or T-40 fiber (AMOCO, tensile strength 5650MPa, 5.1 microns in diameter).

Yoram Sorek
a biological research institute -Ziona, Israel


(2001)

I TOO AM LOOKING FOR INFORMATION ABOUT COATING COPPER ON GRAPHITE FIBERS. LET ME KNOW. THANKS.

VIJAY WANI
a chemical company - MIDLAND, Michigan



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.