I am looking for a way of colouring my brass bullet cases either bright red or blue. The one recipe I have uses potassium chlorate, nickel carbonate & nickel chloride but I can't find nickel chloride and the potassium is too expensive, someone suggested cobalt salts for blue but I don't know where to start. Any help would be appreciated.

Rowan Francis
Bulawayo, Zimbabwe


(1999)

Unfortunately, cobalt salts are a few times more expensive than nickel salts.

Ling Hao
- Grand Rapids, Michigan



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.