Properties of E-coatings




I am a Materials Science student at UCLA, doing a paper on MECHANICAL PROPERTIES OF AUTOMOTIVE ELECTROCOATINGS. I cannot seem to find any values for:

I would appreciate any information on e-coatings. Thank You

Atif Noori
- Los Angeles, California
1999


"Electroplating Engineering Handbook"
by Larry Durney
EEHcover
on eBay
or Amazon
or AbeBooks
(affil link)

You must read chapter 38 of Durney's Handbook.

Do you mean prime coat, top coat, high speed coating of coil stock, two coat systems, ceramic, etc. You may find a supplier's library with a copy of this handbook right in your neighborhood, perhaps even in the your college library.

Best regards,

tom pullizzi monitor   tom pullizi signature
Tom Pullizzi
Falls Township, Pennsylvania


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"