Summary for galvanizing plant consumption Discussion
Water consumption and power consumption in galvanizing plant are not answered with specific figures in the excerpt provided. The page fragment only shows a promotional line for suggested galvanizing books for engineers, shops, and specifiers, including "Faults in Hot-Dip Galvanizing" by Dietrich Horstmann, available in English, French, and German. Because the actual question-and-answer content is missing from the source excerpt, no reliable plant consumption data, formulas, or practical recommendations can be extracted from this page text alone. A reader looking for operating benchmarks would need the full thread or the referenced book sources to find any meaningful discussion of water use, electricity demand, or process efficiency in a galvanizing plant.
SUGGESTED GALVANIZING BOOKS
for Engineers, Shops, Specifiers

“Hot Dip Galvanizing of Steel Structures” by Kuklik & Kudlacek (2016)
avail from
eBay,
AbeBooks, or
Amazon

“Handbook of Hot Dip Galvanization” by Maass & Peissker (2011)
avail from
eBay,
AbeBooks, or
Amazon

“Galvanized Steel Reinforcement in Concrete” by Stephen Yeomans (2004)
avail from
eBay,
AbeBooks, or
Amazon

“Hot Dip Galvanizing — A Guide to Process Selection & Galvanizing Practice” by M. J. Hornsby (1995)
avail from
eBay,
AbeBooks, or
Amazon
“Faults in Hot-Dip Galvanizing” by Dietrich Horstmann (in English, French & German)
avail from
Amazon
“User’s Guide to Hot Dip Galvanizing for Corrosion Protection in Atmospheric Service” by NACE (1997 only rarely avail.)
avail from
AbeBooks, or
Amazon
(as an Amazon Associate & eBay Partner, we earn from qualifying purchases)
Q. Dear Sir / Madam
Hi ..As I found that this site up about finding out the solutions to the seekers…
As we are going to set up a Galvanizing Plant , As everything is at its early stage , So need your help…
As I like to know that what will be the Water Consumption, Power consumption and Area expected in setting up the Galvanizing Plant.
Waiting for your reply
Regards
Pankaj Sharma
Telecom Service provider / Tower manufacturer – Hyderabad, Andhra Pradesh, INDIA
2004
A. Hi, Pankaj. This is a gathering place of camaraderie for metal finishers, so the kind of advice offered would be like what a comrade or friendly competitor might offer you across the dinner table at an educational society meeting. The design of a new galvanizing installation is probably beyond the scope of what you will receive from the readers, and you would need to consult books or retain a consultant for that. But very good luck.