Removing TiO2 Coating
Hi,
I am an undergradute of Nanyang Technological University in Singapore. We are doing some research on TiO2 coating. We encountered problem in removing the TiO2 coating that has underwent heat treatment. Can anyone help?
NG Boon Yong
Nanyang Technological University - Singapore
2004
Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.