Steel thermal treatment before chrome plating
Dear Sirs,
I need information:
I must submit steel -- AISI 431-- to a thermal treatment before chrome deposition; what's the optimal temperature to obtain an iron hardness that guarantees good wear resistance to my chrome layer?
Best Regards
Luca Tosini
Bormioli Rocco - Fidenza, Parma, Italy
2004
Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.