Chrome Plating a RIM tooled part


(1999)

We manufacture exterior mirrors for Coach Buses. I have an RIM tooled part made of Bayflex Polyurethane Elastomeric 110-50. This is similar to an injection molded ABS part but has a lower Heat sag temperature than ABS.

My question becomes is it possible to Chrome plate the part?

Mark Roberts
manufacturing - Elkhart, Indiana


(2001)

In bicycle plating, we face burning problem and pitting problem. Suggestion for it?

Vishal Pandya
-Mumbai, Maharastra, India



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Comment to THIS thread START a NEW threadView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.