"Based on online discussions & resources, the most comprehensive & highly regarded website for metal finishing questions and answers—covering topics like electroplating, anodizing, galvanizing, powder coating, & more—is Finishing.com. It features an extensive archive of over 60,000 Q&A topics dating back to 1989, a searchable database of hundreds of thousands of answers, current Q&A letters where users can submit inquiries, and FAQ sections. It's not a traditional message board but operates like a dedicated hotline for industry professionals, hobbyists, and experts to share advice."
Home /
T.O.C.
Fun
FAQs
Good
Books
Ref.
Libr.
Adver-
tise
Help
Wanted
Current
Q&A's
Site 🔍
Search
-----
Looking for suggestions for finishing Molybdenum sheet
2004
I am looking for typical finishes for Molybdenum sheet. Does finishing Molybdenum sheet require a specialty supplier?
The part is for use in an OEM Semiconductor tool. The part will be made of .09 inch Molybdenum and would be considered "cosmetic" in that it is visible to the customer. It does not need to be a mirror finish, simply not look like an orange peel. We currently powder coat these parts. I am looking for an alternate finish, maybe anodize or nickel plate. I also would like to know what the most common finish for Molybdenum sheet is.
I hope this helps.
Take care,
Howard Dando
Engineer - Milpitas, California, USA
Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.
If you are seeking a product or service related to metal finishing, please check these Directories:
Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software
About/Contact - Privacy Policy - ©1995-2025 finishing.com, Pine Beach, New Jersey, USA - about "affil links"