topic 32895

Carlo De Giorgi electroplating equipment manual or knowledge


2004

I'm trying to find out if anyone has any experience with Carlo De Giorgi electroplating equipment. I purchased a like new 4000 Light model (beaker type) but I cannot find any information on it or any type of manual and don't have a clue how to use it. I have tried the internet and have located the company but as far as I can tell they only deal in dental equipment now.

Brian Bonser
Gunsmith - Stuart, Florida, US



If you have a question in mind which seems off topic, please Search the Site

ADD a Q, A, or Comment on THIS topic START an UNRELATED topicView CURRENT HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2019 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.