I am looking for possible solutions for coating an aluminum alloy. The substrate can be up to 47" long. Corrosion resistance, cost, and weight are all big factors in our application.

Kenny Rump
- Memphis, Tennessee


(1999)

If you're looking for corrosion resistance only with low weight and low cost try IVD aluminum. Large parts are not a problem -- typical deposition chambers are 8 to 12 feet long.

jim treglio portrait
Jim Treglio
- Vista, California


(1999)

Hi Kenny , You really need to provide us with more information , what kind of environment the products will be exposed to , (i.e., , domestic interior , industrial exterior , motor car , under hood or underbody ? all have different needs ) But a good coating on Aluminium is Anodising and it can be specified in different ways & thicknesses to achieve your specific requirements . Broaden your question and we may be able to help further regards

John Tenison-Woods
John Tenison - Woods
- Victoria Australia


(1999)

What sort of volume are you talking about? What kind of environment would the coated part encounter?

Charles Baldwin
- Cleveland, Ohio


(1999)

I m working in aluminum alloy anodized and I think that the thickness layer have a influence in life fatigue,but I don't have explanation about this. Pedro Paulo

Pedro Paulo de Campos
- Sło Jose dos campos sao paulo BRAZIL



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.