Plating on Plastics


(1999)

Seeking literature on plating on plastics specifically electroless, or electrodeposited deposits of copper, or nickel onto basic plastics such as thermosetting (epoxies, phenolics, polyesters, etc.) and thermoplastics (acrylics, fluorocarbons, polyesters, polysulfones, etc.).

Tom Andersen
- Balto., Maryland


(1999)

Hi Tom, I use a process from Fidelity for plating onto all types of non-conductors. It seems to work very well, although I only have a small benchtop line. The name is Ultraplate and they may send you a sample of it. You can give me a call if you like also.

jim conner
Jim Conner
Anoplex - Dallas, Texas USA


(2000)

Letter # 3384 was addressed by a Jim Conner of Salisbury, MD

I am interested in Plating Phenolic Plastic, Jim said that "Ultraplate" works. I can't seem to locate a company called Ultraplate that does this process. Can you help?

Kevin Emmett
- N. Tonawanda New York


Ed. note: Jim was apparently saying that Ultraplate is a product of Fidelity [Chemical Co., Newark, NJ], Kevin.



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.