Surface finish for IMP parts


(1999)

I ran into an old print for an injection molded plastic part that specifies an SPI No.6 finish for the surface. I would like to know where I can find a complete list of specifications for surface finishes on IMP parts that includes the one mentioned earlier.

Samuel Ocampo
- Columbia, Maryland


(1999)

There is no better source than the person who signed the print.

tom pullizzi monitor
Tom Pullizzi
Falls Township,
   Pennsylvania 


(2001)

Same question: do you know if any on-line tables/lists/examples of mt and spi finish specs?

Thanks,

Chris Tesluk
- Mansfield, Massachusetts



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView This Week's HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.