Chrome plating apparatus


(1999)

Hello!

Does anyone know any companies who manufacture smaller chrome plating apparatuses? I have found one [Cronite Co., Parsippany, NJ ] but I was wondering if there are anyone else. I need one to plate copperplates of engravings/etchings when print runs exceed 300-400 copies. Maximum plate size 15 x 20" or so.

In Sweden, regulations are strong, but not as strong as in US, apparently, so it is feasible,

Mats Broberg
- SWEDEN


(1999)

I am only partially familiar with your use. I do not think that chrome is a viable candidate for plating copper as is is so smooth that it will not hold ink evenly. It will tend to ball up like a water drop on a highly polished hood of a car. One lady that I worked with recently was using iron plating for exactly what you described. Am I wrong in your case? Jim

James Watts
- Navarre, Florida


(1999)

I would think that your best approach would to be to buy a small, self-standing polyethylene or polypropylene tank rather than a custom built system. Chrome plating is a relatively easy process and doesn't take elaborate equipment.

Using chrome to plate copper printing plates is a very common practice in the rotogravure industry and done when they anticipate 1M impressions or more. Figure on putting on 0.001 to .015" if you're expecting some real high printings. The use of a fluoride chrome bath might be of good use to ensure plating down into the "pits" and "grooves" of your plates. Hope this is of some help. I was formerly a chrome plating sales/service specialist with Diamond Shamrock years ago and still work with platers on chrome problems. Don't think I'd consider iron plating-not a very common plating medium. Best regards, Bill Parthe


William Parthe
- Garrettsville, Ohio



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.