topic 3122

Tungsten plating


1999

Dear Friends, Is there information available for plating Tungsten on steel or aluminium ?

TJ Sharpe
- Lewisville, Texas


1999

Hi TJ

Pure tungsten cannot be deposited from a conventional aqueous plating bath. Your options include codepositing it from a cobalt or other plating bath, plating it from an organic or molten salt electrolyte, or using some vacuum deposition process. Good luck.

Ted Mooney, finishing.com Teds signature
Ted Mooney, P.E.
finishing.com
Pine Beach, New Jersey



If you have a question in mind which seems off topic, please Search the Site

ADD a Q, A, or Comment on THIS topic START an UNRELATED topicView CURRENT HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2019 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.