-----Want General Chemical Resistance Chart for EN Plating
I am looking for a chart that shows general chemical compatibility with electroless nickel plating. Things like common acids, bases, gasoline and other petrochemicals, Freon, etc...
Gary Harrisquick connect couplings - St. Paul, Minnesota, USA
2004
2004
Some corrosion resistance data is included in Riedel's book, Electroless Nickel Plating (ASM International, Metal Park, OH, 1991). A more complete listing is in Duncan's paper, Corrosion Resistance of High Phosphorus Electroless Nickel Coatings, which was presented at the Third AESF Electroless Plating Symposium in Orlando in 1986 (American Electroplaters and Surface Finishers Society, Orlando). This paper was also summarized in the magazine Plating and Surface Finishing (Vol 73, No 7, 1986, published by the AESF).

Ron Duncan [deceased]
- LaVergne, Tennessee
It is our sad duty to note Ron's passing on Dec. 15, 2006. A brief obituary opens Episode 13 of our Podcast.
Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.