Please give me formulation of carbon stop off compound for selective carburising or anti carb.
Naresh Agarwalplating shop - Ranchi, India
2004
Copper electroplating is a common and often practical approach.

Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
Need quick confidential answers? $25
Need project assistance? $100/hr.
2004
Ref book you can use enamel coating a sample-SiO2/72%V-al2o3/1.5%v b2o3/1%v-MgO/2%V-CaO/5%V-NaO+K2o/16%v-PbO/2%V-STAND UP TO 650-850 °C. You can use aluminum, copper coating.
Good luck

Khair Shishani