Nickel or copper coated graphite powder


(1999)

I am a student in graduate school. I study modeling of melted Al. I need Ni-coated graphite powder or Cu-coated graphite powder. The size of powder is 10-200 micrometer, but size must be constant. If you have information or powder, I wish you'd send mail. Please .... I need powder .... not products. Have a nice day.

Jongmin,Lee
- Seoul,South Korea


(1999)

The best source of this type of powder that I know of is probably the Acheson Colloids [Port Huron, MI] Electrodag range.

Rob Legg
- Melb, Australia


(1999)

There are two companies that I know of that coat nickel on graphite powders: Novamet Specialty Products [Wyckoff, New Jersey] and Westaim Specialty Products Edmonton, Alberta Canada. Hope this helps.

Dave Greenwood
- Lowell Massachusetts


(1999)

As you are a graduate student, I want you to know that nickel and copper coated graphite powder is a product. You need to specify what you mean by "constant" size. For instance, an average diameter, with a standard deviation?

It is a very specialized product, the production of which has already taken up thousands of man-years of effort, and as new uses are discovered for it, thousands more.

Regards, Tom

tom pullizzi monitor
Tom Pullizzi
Falls Township,
   Pennsylvania 


(2001)

I am a student in graduate school. I study on metal-graphite electrical brushes. I need information on Cu-coated graphite powder.

Have a nice day.

Ibrahim Yasar
- Trabzon, Turkey


March 9, 2008

Hi
I am Yerriswamy W Asst.Prof., doing Research on the topic 'COATING OF GRAPHITE' by using copper (Electroless plating) 100-200 microns size. Please mention the aim of your study by using same. Coated graphite of your specification is available
With Regards

Yerriswamy Wooluru
- Bangalore,Karnataka,India



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView This Week's HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.