Dear sirs, I am a Project Engineer for a rapidly growing construction company based in SLC, Utah. We now have GC licenses in Utah, California, Arizona and are in the process of obtaining licenses in Nevada, Oregon and Washington. I am trying to find all of the technical information I can find on the powder coating process. Specifically the cost, ease of application and durability of powder coating vs. polyurethane enamel for outdoor steel structures subjected to fairly harsh seasonal changes. I would appreciate any and all help on this matter. Thank you, Craig Rasmussen

Craig Rasmussen
construction - Salt Lake City, Utah


(1999)

Dear Mr. Rasmussen Ask Emma Scham of Protective Coatings Europe, to send you a reprint of PCE Issue February 1999, pages 18 - 23. This is an article about powdercoating steel structure for outdoor use. Tell her I gave you her name, Best regards,

Remmelt Bosklopper
Remmelt Bosklopper
- Enschede, The Netherlands


(1999)

I'll suggest several possible sources of help: The Powder Coating Institute. The Suppliers Pages of finishing.com (powder coat suppliers).

Good Luck,

Craig Burkart

Craig Burkart signature
Craig Burkart
- Naperville, Illinois




This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.