I would like to obtain information concerning the different tecniques of finishing galvanized sheet metal products. I would be interested in the areas of changing the color as well as a product to "age" it without damaging the finished surface. Please contact me if you have any information to help me with this project. Thank you

Cherri
- Protem, Missouri


(1999)

Dear Cherry. The best way of "Aging" galvanized sheets is by putting them is SALT SPRAY CABINET , an instrument that measure the corrosion standing ability . I used to do it with copper parts that they will appear very old as antiques. Yours Yehuda

yehuda blau
Yehuda Blau
YB Plating Engineering and Quality - Haifa Israel



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.