topic 2948

I need help with a masking problem.


(1999)

We have a simple problem...We are powder coating some threaded steel pipe. We mask the threaded ends with tape. The tape is hard to remove and the exposed theads quickly rust! We are looking for a better way and would welcome your suggestions. Ed Smith Quality Engineer

Ed Smith
- Clovis CA


(1999)

Look into cap plugs made out of high temp material. There are numerous advertisements for them in the Metal Finishing Guidebook.

James Watts
- Navarre, Florida



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.