IVD Peel Strength


(1999)

I am interested in the peel strength of IVD aluminum coatings on aluminum substrates. Any replies would be greatly appreciated.

Jeremy Green
- Dallas, Texas


(1999)

The strength should be as good as the tensile strength of the aluminum if done properly.

Donald M. Mattox
Society of Vacuum Coaters
Albuquerque, New Mexico

Ed. note:
            Mr. Mattox is
            the author of -->



June 9 -

Here at our shop we coat a variety of aluminum alloys with IVD Aluminum. For a peel test, we use 3M tape #250 on the IVD Aluminum. This #250 tape has a peel strength of 62 lbs PSI.

Jerry Wahlin
plating shop - Compton, California



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView This Week's HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.