Brass plate 800 lb bell?


(1999)

I am looking for a brass plater with the capability of plating an 800 poound bell. The bell is approximately 4 feet tall and 3 1/2 feet wide. The owner of the bell lives in Saling Michigan.

Jonas McCluskey
Plating Company - Jackson, Michigan


(1999)

- Dear Jonas , I would think that this is a perfect job for a "Brush plater". Best regards

John Tenison-Woods
John Tenison - Woods
- Victoria Australia


(1999)

John Tenison is correct that brush plating would work well on this project. The part can be done on site or in a shop, which gives you more versatility.

David Crocker
- Valencia, California



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.