Stripping NiP and Cu from Zinc Diecastings


(1999)

We are having problems (parts are not properly coated) with electroless nickel plating of zinc diecast with an undercoat from cyanide copper baths. How is it possible to chemically strip the NiP/Cu layer system without attacking the zinc diecast base material.

Franz-J. Stark
Kerpen - Germany


(1999)

Metalx [a finishing.com supporting advertiser] sells a stripper that removes nickel from copper and zinc die cast. I do not know if it will work on EN. It might if it were jumpstarted. They could tell you. I have not used this particular product, but I have used a different one of this family of B-9 strippers and it is the best of several that I tried. Nice people and a very small company.

James Watts
- Navarre, Florida


(1999)

Please also see our FAQs on Stripping of Electroless Nickel.

Regards, Ted Mooney, finishing.com Teds signature
Ted Mooney, P.E. RET
finishing.com
Pine Beach, New Jersey



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView This Week's HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.