Stripping NiP and Cu from Zinc Diecastings




We are having problems (parts are not properly coated) with electroless nickel plating of zinc diecast with an undercoat from cyanide copper baths. How is it possible to chemically strip the NiP/Cu layer system without attacking the zinc diecast base material.

Franz-J. Stark
Kerpen - Germany
1999


Metalx (Ronatec.us) [a finishing.com supporting advertiser] sells a stripper that removes nickel from copper and zinc die cast. I do not know if it will work on EN. It might if it were jumpstarted. They could tell you. I have not used this particular product, but I have used a different one of this family of B-9 strippers and it is the best of several that I tried. Nice people and a very small company.

James Watts
- Navarre, Florida
1999



1999

Please also see our FAQs on Stripping of Electroless Nickel.

Regards, Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.


adv.
Metalx nickel stripper

Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"