Home of the finishing HOTLINE since 1989

-----

Titanium plating on steel products like manicure items





I just need to get the complete process for the electroplating of titanium on the stainless steel and also on the carbon steel; kindly help me out of this as I am really in need of that. Looking forward to have the favorable answer for that.

Regards,

AHSAN UL HAQ
Proprietor - DUBAI, UAE
2004



It is generally accepted that titanium is not commercially electroplateable, although our friend Goran Budija has been kind enough to give us some formulas from plating books for laboratory attempts. You may be actually seeking titanium nitride finishes--the color they put on "gold" drill bits? These are applied by PVD processes, so you would need to install the PVD equipment or retain the services of a jobshop that offers it.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.
2004


Titanium Coating is a Big process and not like ordinary electroplating. It is called PVD coating. Huge machineries required for that.

D GEORGE
- DUBAI, U.A.E.
2007


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"