Vibratory Plating


(1999)

Does anyone have any experience using a vibratory plating machine to nickel coat material having a size of 100/120 mesh and smaller? Thank you.

warren silverman



I can't tell you too much about this, Warren, because the company I'll mention is as much about intellectual property as about offering product for sale, but I would suggest that you contact:

Dr. David Lashmore
Research Director
Materials Innovation
8 Commerce Avenue
West Lebanon, New Hampshire 03784
Ted Mooney, finishing.com Teds signature
Ted Mooney, P.E. RET
finishing.com
Pine Beach, New Jersey



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.