Electropolish racking problem


(1999)

We are starting out on electropolishing of stainless steel spoons. We are having problem with holding the articles tight. This resulted in arcing of the spoons. Can anyone assist by telling us best to hold the spoon with so that only a small surface is shadowed and the spoon does not arc when it is rocked about?

We tried using titanium clip, not unlike the hairpin.

Do you think a more positive contact like wing nut and screw would solve the problem?

Steven Chen
- Auckland, NEW ZEALAND


(1999)

Steven: Titanium has good chemical resistance to the bath, but that metal does not carry enough current for most electropolishing applications. Try copper or phosphor bronze contacts. Regards, Ed Bayha

Ed Bayha
Metal Coating Process Corporation - Charlotte, North Carolina


(1999)

At our company we do a lot of electropolishing so it might be possible that I could be of some assistance. To make things a bit clearer: Why don't you send me an E-mail with a drawing/explanation attached showing your racks and how the spoons are placed.

Hans Henrik Larsen
- Odense, Denmark

---

Ed. note: Better yet, Steven, send the drawing here and we'll post it for all to see. Although it's nice for people to offer personalized replies, taking a public discussion to private email would disenfranchise hundreds of readers whose curiousity has been aroused.



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.