PU thinner formulation: useful answer on standard mix

Summary for pu thinner formulation Discussion

PU thinner formulation is the focus of this short thread, where the questioner asks whether there is a standard recipe for manufacturing thinner for PU (polyurethane) paints. The excerpt provided does not include any technical replies, formulas, or named expert guidance, so the page appears to be an unanswered request for a standard formulation rather than a solved discussion. Based on the available text, the only clear takeaway is that the user is seeking a thinner suitable for PU coatings used across all products, but no answer in the source confirms a universal mix or recommends specific solvents. Because no response text is present, no further technical conclusion can be drawn from this thread excerpt alone.

Q. We are painting all our products with PU paints. Is there any standard formulation available for PU thinner manufacturing.

Regards,

Xylene

xylene

on Amazon
or


eBay


(affil link)

T.Raj Mohan Doss
Engineering product – Hyderabad, Andhrapradesh, India
2003

A. Xylene

⇦ on

eBay

or

Amazon [affil link] 55

Cellosolve acetate (CA) ⇦ on

<!–
eBay or
–>

Amazon [affil link]

35

Butyl acetate (BA) ⇦ on

eBay or

Amazon [affil link]
15

Try this formula, and please tell me the result

Andrea Djaja
– Semarang, Central Java, Indonesia


“Polyurethanes: Science, Technology, Markets, & Trends”

pu_formulation

on Amazon

or

eBay

or

AbeBooks


(affil link)

“Polyurethanes: Coatings, Adhesives & Sealants”

polyurethanes

on Amazon

or

eBay

or

AbeBooks


(affil link)

Q. Respected Sir,

I am a Recent graduate of Chemical Engineering.

I am planning to start a small scale thinner Manufacturing business.

please help me out in getting the formulations for Degreasing/Flushing/Cleaning Thinner.

Hoping positive reply from you !

Thanking you !

Mohammad Feroz
– Kuala Lumpur, Malaysia
November 18, 2011

Q. I am trying to start manufacturing 2K automotive refinishes. Can someone give me formulation of it?
I think it would be acrylic resin based.

Shahed Sultan
– Chittagong, Bangladesh
March 9, 2012

Q. I am a Recent graduate of Chemical Engineering.

I am planning to start a small scale thinner Manufacturing business.
Can someone help me out with PU thinner formation.

ALVIN JOHN
– THRISSUR, Kerala, India
July 19, 2013

Q. Respected Sir,

I am a Recent graduate of Chemical Engineering.

I am planning to start a small scale thinner Manufacturing business.

please help me out in getting the formulations for Degreasing/Flushing/Cleaning Thinner.

Hoping positive reply from you !

Thanking you !
Rubel from dhaka bangladesh

Md.Rubel Mia
Etc – Dhaka, Bangladesh
October 17, 2024