Cloud-Chamber coating process


(1998)

I am looking for information on a variation of the vacuum-coat process called a "cloud-chamber" where coating is supposedly atomized to form a "cloud" whereby coating parts. Has anyone heard of this process and if so do you have info. on equipment?

David C. Jones
- Charleston, South Carolina


(1998)

We have developed a vapor-cloud type method for vacuum metallizing but we do not call it vapor-cloud; we call it vapor-bath. I wonder if that is what you are referring to.

Mandar Sunthankar
- Fort Collins, Colorado



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.