Hello:

We produce rack mounted audio/video equipment for the broadcast industry. I would like to know which has the best conductivity and to what degree are the differences, between zinc with clear chromate, yellow chromate, and black chromate. Are their any differences in the corrosion resistance of the three. We need the best electrical grounds for EMI.

Thanks
Don

Don Hudson
- Salt lake City, Ut


(1998)

Don,

Because the chromating conversion coatings are very thin, they are all conductive. However, clear chromate film has relatively low electric resistance since it is thinner than yellow and black chromate films. On the other hand, yellow and black chromate coatings offer much better corrosion resistance than clear chromate coating.

Ling

Ling Hao
- Grand Rapids, Michigan


February 28, 2011

I agree with the statement in regards to all three chromates being conductive, but is this true for the new wave of Tri Chromates as well?

Abel Salazar
anodizing and plating - Anaheim, California, USA



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView This Week's HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.