Would like to make a gold plating solution with potassium cyanide for plating gold or stainless steel. Please help me make the right solution, as I have tried to but it does not work as it should. Any one can help?

Daryanani Nik
jewelry


(1998)

Dear Nik ,

Without a better description of what "didn't work" I am afraid I would be only guessing , however , there is a wealth of information and service available from people such as Technic who specialise in Gold plating proprietary chemistry , give them a call , don't try to reinvent the wheel !

regards

John Tenison-Woods
John Tenison - Woods
- Victoria Australia


(2000)

Enthone-OMI has a special gold-strike to plate gold directly on stainless steel.

Willy Desmadryl
- Belgium



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView This Week's HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.