Silver or gold coatings on glass


(1998)

Dear Sirs,

I am looking for a supplier being able to make silver or gold coatings on glass for soldering. Is this your field of expertise ?

Best regards,

M. Kautz
- Jena, Germany


(1998)

Herr Kautz,

In the vacuum deposition industry this is commonly done by depositing a "glue layer" of titanium or chromium on the glass followed by a soldering layer of copper with perhaps a flash of gold. Look for someone doing contact coating by vacuum deposition in you area. One group is Tricon GMBH in Freiburg, Germany.

Donald M. Mattox
Society of Vacuum Coaters
Albuquerque, New Mexico

Ed. note:
            Mr. Mattox is
            the author of -->




This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView This Week's HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.