BASIC PRIMER ON ANODIZING?


(1998)

Looking for a basic primer on anodizing. How to do it in my shop. Need help with all aspects. Thanks much!

Ed Janssen


(1998)

The best book that I have seen is Light Metals Finishing Process Manual by C. Grubbs and D. Montgomery. You get it thru American Electroplaters and Surface Finishing Society.

Relatively simple, fairly complete and decently priced.

James Watts
- Navarre, Florida


May 13, 2008

Hi, Ed. I have the book that James talks about and I share his view towards it. But it is becoming frustratingly difficult to locate a copy these days, and I think Robert Probert's "Aluminum How-To" is quite similar from the points of view of "simple, fairly complete, and decently priced".

Regards,

Ted Mooney, finishing.com Teds signature
Ted Mooney, P.E.
finishing.com
Pine Beach, New Jersey



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.