Deburring small stainless and titanium parts


(1998)

I am interested in information on deburring small stainless and titanium parts. Does anyone know of any conferences and/or seminars that would help me?

Harv Hornung
- Clarence, New York


(1998)

Mr. Hornung,

If its a seminar you're after, check with SME (Society of Mfg. Engineers). They do a 2-3 times/year seminar on Mass Finishing. I've been to it and it is a good overview on what you are trying to learn. You can contact SME at their customer service center. They should be able to help. Good luck.

Dan Regan
mechanical prep specialist - Cinnaminson, NJ



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView This Week's HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.