finishing.com -- The Home Page of the Finishing Industry
A website for Serious Education, promoting Aloha,
& the most FUN smiley you can have in metal finishing

HomeFAQsSuggested
Books
Help
Wanteds
Advertise
Here
FORUM
(current
topics)
topic 2205

Electroforming Magnetic materials


(1998)

I am interested in learning if anyone has done any electroforming of magnetic materials (in the range of 6-8 mils). Are there any alloys possible, or other materials? Thanks.

Patricia J. Frisch



Yes, Ms. Frisch, there are a number of magnetically hard and magnetically soft metals and alloys that can be plated. The MFIS CD-ROM showed more references than I had time to look up, probably 50 good references. Are you looking to make a permanent magnet or something softer?

Ted Mooney, finishing.com Teds signature
Ted Mooney, P.E. RET
finishing.com
Pine Beach, New Jersey


(1998)

Where could I get a copy of the MFIS CD-ROM, and how much does it cost?

Patricia J. Frisch



(2002)

Finishing.com now distributes this, and you can order on-line. Current cost is $295.

Ted Mooney, finishing.com
Teds signature
Ted Mooney, P.E. RET
finishing.com
Pine Beach, New Jersey

Ed. note 2008: Finishing.com no longer handles the CD-ROMS because it became an on-line service. Look up "Metal Finishing Information Service" in England.



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.