| Search our quarter-million Q&As |
Home of the finishing HOTLINE since 1989
-----MIL-C-5541 Class 3
Dear Sir, we are currently looking for MIL-C-5541 Class 3 Type. I only can find the MIL specification information, but no cross-reference to any product. May it be possible to send a cross reference list between MIL-C-5541 Class 3 to the common used product. Within your information (Questions and Answers) I only found the
Iridite, but there should be another type of coating being reference to.
Thank you for your help.
Best Regards,
airline - Cologne NRW, GERMANY
2003
Hello, Mr. Weidenbrueck
There is a separate spec, the "Qualified Products List",
QPL-81706
[⇦ this spec on DLA] which lists the products which are qualified to be used in Mil-C-5541 chromate conversion coating, including Iridite and other trade names.

Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
Need quick confidential answers? $25
Need project assistance? $100/hr.
2003
Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!