Why is it important to electroplate metals?

Jessi G. [surname deleted for privacy by Editor]
- Dallas, Texas, United States
2003



Take a couple of guesses and then I'll be happy to help you out, Jessi. But just taking 30 seconds to post your homework assignment on-line for somebody else to do for you is inappropriate.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.
2003



This question is very rough. We electroplate metals for numerous reasons: as for wear resistant, corrosion resistant, oxidation resistant, decorative applications and etc. Should see what application you need from electroplating?

Thanking you,

S. R. Bakhshi
- Isfahan, Iran
2003


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"