How to dissolve Tin Oxide


Q. The question I had is that; What do you use to dissolve Tin Oxide in a microwave?

If anyone know that method, please let me know.

Thank you.

Su Kue
Umicore Indium Products - Providence, Rhode Island, USA
2003



Q. PLEASE GIVE ME THE ANSWER OF ABOVE QUESTION "HOW TO DISSOLVE TIN OXIDE" AS SOON AS POSSIBLE.I SHALL BE VERY THANKFUL TO YOU.

Arham Shareef
A.M.U - India
July 10, 2008


A. Best bet: SnO2 + 2 H2SO4 ⇨ Sn(SO4)2 + 2 H2O

nef erata
- brisbane qld australia
September 22, 2014


Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"