Copper plating titanium nitride


(1998)

I am currently trying to copper plate TiNi and am having a problem with adhesion at the interface. The solution I am using is an acid bath, at a low current density, and a copper electrode from a commercial acid bath.

How can I get a better adhesion?

I have already tried annealing and pumping argon through the bath.

Gabriel Wright

(1999)

Hi, I'm working as process eng,for plating processes and I will be interested to exchange opinion and experiences.

Paolo Alagna
- Kalispell MT



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.