-----Industrial testing standard on Dacrotizing
1998
In addition to the 5% salt spray testing (ASTM
ASTM B117 ) on "Dacrotizing"; does there exist any "industrial standard" such as "JIS , ASTM ,.." on "Dacrotizing"?
Thanks a lot
Fong Prean industrial .,co.ltd - kaoshiung , Taiwan
1998
Dear Mr. Cheng,
In the US,ASTM B117, MIL
C-87115A, MIL:S-001222G
British standard,
BS 7371-11
No JIS.
Almost all major automobile makers in the world have specification on DACROTIZING and also many other industries.