Home of the finishing HOTLINE since 1989

-----

Zamak, finishing collinox 1010

I am a materials engineer and I need some information about a finishing treatment applied on zamak alloys named "collinox 1010".

Antonio Florio Filho
- Maua, Sao Paulo, Brazil
2002



Dear Antonio Florio Filho,

I'm R & D engineer diecast company in Korea. I need also information about a finishing treatment applied on zamak alloys "collinox 1010" so I request information from you. If you have information. I not very well English but I believe you understand.

Thanks and best regards,

Inwoo Choi
- Inchon, Korea
2003



I'm engineer and I need information about collinox 1090. Thanks,

Gemma

Gemma Gascón
engineer - Spain
March 21, 2011



Hi, folks.

Collinox (there is a double l) is a trade name of the Collini group, with 13 locations in Europe. Good luck.

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.
March 21, 2011


Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"