Electrowinning Cell Vendors


(1998)

I am looking for some electrowinning cell (or system) vendors to recover copper from a spent copper sulfate plating bath. Can you recommend any suppliers from the West (near California)?

Thanks in advance for your help.

b maeda
-California


(1999)

I was after some information on modelling electrowinning cells, namely optimum current densities for paticular tenor grades and cell volumes. A reference or any info would be appreciated

nigel grigg
Australia


(1999)

I am looking for some information on modelling electrowinning cells, (wherein simultaneous deposition of metal at cathode and EMD at anode can be possible) , namely optimum current densities for paticular tenor grades and cell volumes, etc.. A reference or any info would be appreciated

v misra
- New Delhi


(1999)

ElSyCa and L-Chem [Beachwood, OH] are two suppliers of such modelling software.

Ted Mooney, finishing.com Teds signature
Ted Mooney, P.E.
finishing.com
Pine Beach, New Jersey


(2002)

Mr. Grigg,

At the moment I am developing to a project with the group of investigaciones of Minerals, Biohidrometalurgia and Ambiente. Found in Internet an articulate of which you is the author about intensive cyanidation and electrowinning, him agradeceria if it sent but information about this subject.

Thanks for the lent attention.

Senor Grigg,

En el momento estoy desarrollando un proyecto con el grupo de investigaciones de Minerales, Biohidrometalurgia y Ambiente. Encontre en internet un artÌculo del cual es ustede el autor sobre Cianuracion intensiva y Electrodeposicion, le agraceceria mas informacion acerca de este tema Gracias por la atencion prestada.

Jenny Rocio Gutierrez Pitta
Grupo de Investigaciones en Minerales, Biohidrometalurgia y Ambiente. UIS - Bucaramanga, Santander, Colombia



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.