Krytox lubricant films


(1998)

Does anyone have experience in fusing Krytox® (duPont) Teflon® lubricant films to surfaces? I would like to know the optimum heating rate, temperature and time at temperature for maximum durability of the film on the surface.

Donald M. Mattox
Society of Vacuum Coaters
Albuquerque, New Mexico

Ed. note:
            Mr. Mattox is
            the author of -->



September 9, 2010

I've done work with KrytoxDF/HCFC and KrytoxDF/W with metal and plastic components. What type of Krytox are you using and with what materials?

diane icard
- Batesville, Ohio


January 26, 2011

Dupont has now come out with a powder form of the teflon substance where it only requires heating to melt the surface to to substrate

Diane Icard
- Batesville, Indiana



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.