Can you recommend an economical coating (paint, plating, etc.) process for use on a zink alloy casting (ZA-8)? This part needs to be black for appearance only.

Patricia J. Volpe
Sears Manufacturing


(2000)

I too am interested in painting new zinc castings with a spray-applied coating (black). Has anyone found a cleaner/primer/paint sequence which was successful?

Ernest Cox
APEX Industries


(2003)

Is there a way to spray zinc on parts to achieve a uniform even coat?

James Gagne
Vangaurd Building Systems Inc. - Wells, B.C.



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.