(1998)

The framework is manufactured by welding Al tubes to form the structure. Is there any way to clean the joints and the tubes to a bright finish (like an ANODIZED surface) and then coat it for scratch protection ?

Thank you for your guidance !

Ashwin P. Badve
- Micro Metals, Inc.


(1998)

I'm assuming this rail is already installed on a boat. Your best bet is to purchase about 6 Black & Decker buffing wheels from your local hardware store, red tripoli [link to product info at Amazon by ed.]; put the 6 buffing wheels on a portable grinder shaft and buff the aluminum rail. I estimate approximately 30 minutes per 1 ft. of rail. Be sure to wear the appropriate safety clothes. If you need any more help contact a local metal polishing shop.

Gary Patigler
Richmond, California



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.